My Metallic Floor Failed 4 Months After My Install
Hello, I hope everybody is doing well today. I am just getting here to see if anybody has any information or experience with something similar to what’s been happening unfortunately I have my first Epoxy Flor failed on my career. This floor was performed with moisture barrier. Follow up with the metallic design everything coming up very good And four months and a half later customer called me and say hey my floor start getting some bubbles so I went out and I’m gonna attach a few files right here for y’all to look at. When I date my moisture reading with the {CMEX5 } my reading was 0.4 CONCRETE MC. Now I want to be clear not the entire floor is failing this is happening only 29 inches from the exterior wall perimeter into the interior slap. Everything else is in good shape.
1:16
0
6 comments
My Metallic Floor Failed 4 Months After My Install