125 amps-struggled on the pedal with heat at the end of runs.
150 hertz
3/32 2% lanthanted tungsten
1/8” 4043 filler rod.
#6 cup on 18-19 cfh
I did clean up the corners before I gave it to a co worker. I also have a video of all welds. Had to cut out two of them and redo them so they got a little wider and grainy.